1Postgraduate, Department of Prosthodontics & Crown and Bridge, Manipal College of Dental Sciences, Mangalore, Manipal Academy of Higher Education, Manipal, Karnataka, India
2Professor and Head, Department of Prosthodontics & Crown and Bridge, Manipal College of Dental Sciences, Mangalore, Manipal Academy of Higher Education, Manipal, Karnataka, India
3Associate Professor, Department of Prosthodontics & Crown and Bridge, Manipal College of Dental Sciences, Mangalore, Manipal Academy of Higher Education, Manipal, Karnataka, India
4Professor, Department of Prosthodontics & Crown and Bridge, Manipal College of Dental Sciences, Mangalore, Manipal Academy of Higher Education, Manipal, Karnataka, India
5Assistant Professor, Department of Prosthodontics & Crown and Bridge, Manipal College of Dental Sciences, Mangalore, Manipal Academy of Higher Education, Manipal, Karnataka, India
Online published on 27 November, 2019.
The aim of the study was to evaluate and compare the shear bond strength of porcelain repair system using Ni-Cr and Co-Cr alloys.
Thirty discs of base metal alloy were fabricated and divided into 5 subgroups Control, Roughened with the diamond point, Air abrasion/Sandblasting Hydrofluoric acid treatment, Phosphoric acid treatment. Shear bond strength testing and mode of failure was evaluated using ANOVA and Post Hoc Tukey Test,
The least bond strength was seen in the control group and the highest in Air abrasion followed by hydrofluoric acid.
Use pf intraoral porcelain repair may be considered as the viable and economical treatment option,
Intraoral, ceramic repair