Indian Journal of Public Health Research & Development
  • Year: 2018
  • Volume: 9
  • Issue: 9

Effect of surface finish on stain affinity of a lithium disilicate esthetic ceramic material

  • Author:
  • Nikita Batra1, Shobha J Rodrigues2,, Sharon Saldanha3, Thilak Shetty4, Umesh Pai5, Mahesh Mundathaje5, N Srikant6
  • Total Page Count: 6
  • Page Number: 303 to 308

1Postgraduate Student Department of Prosthodontics, Manipal College of Dental Sciences, Manipal Academy of Higher Education, Mangalore, India

2Professor & Head, Department of Prosthodontics, Manipal College of Dental Sciences, Manipal Academy of Higher Education, Mangalore, India

3Associate Professor, Department of Prosthodontics, Manipal College of Dental Sciences, Manipal Academy of Higher Education, Mangalore, India

4Professor Department of Prosthodontics, Manipal College of Dental Sciences, Manipal Academy of Higher Education, Mangalore, India

5Associate Professor, Department of Prosthodontics, Manipal College of Dental Sciences, Manipal Academy of Higher Education, Mangalore, India

6Professor & Head, Department of Oral Pathology, Manipal College of Dental Sciences, Manipal Academy of Higher Education, Mangalore, India

*Corresponding Author: Dr Shobha J Rodrigues Pofessor & Head, Department of Prosthodontics, Manipal College of Dental Sciences, Manipal Academy of Higher Education (MAHE), Mangalore, Email: shobha.j@manipal.edu

Online published on 25 September, 2018.

Abstract

To evaluate the influence of two different surface treatments on the stainability and color change of ceramic restorations.

veneering lithium disilicate was used to fabricate standardised discs (n=60). These discs were abraded using a red band diamond abrasive. Samples were divided in three groups. Surface Roughness (Ra)values before and after the surface treatment were calculated using a surface profilometer. These specimens were further subdivided into 2 subgroups with 10 samples each. Colour change (δE) values were calculated at 6, 12, 18 and 24 days.

Independent t test for the groups Polish and Reglaze showed a significant difference (p = 0.003). One way ANOvA for the Green tea group showed a significant difference (p = 0.007) at 12 days between Control and Polish and Control and Reglaze. One way ANOvA for the Turmeric group showed a significant difference at 12, 18 and 24 days.

For increased periods of clinical usage corresponding to increased immersion times, reglazing was necessary to prevent stain absorption especially against Turmeric.

Keywords

Color stability. emax Press. Turmeric. Green Tea